L6
On 2017-08-14 10:11 am, Ron Childers wrote:
> I have a piece of old band saw blade without carbide teeth, probably from a Wood Miser. What kind of steel is it likely to be? 15N20 maybe? What steel is used in circular saw blade that has carbide teeth? Thanks, Ron