thanks Mike. That was the plan all along but thanks for your input...
dave m
On Thu, Mar 10, 2016 at 3:43 PM, Mike Spencer <mspencer at tallships.ca> wrote:
>
>
> I'd just add what's obvious: Get a moderately massive scrap of the
> same alloy from your client and try your MIG settings and chosen
> filler on it. Then you won't have any major surprises when you hit
> the big gear.
>
> (Err... that *is* obvious, isn't it? :-o )
>
> - Mike
>
> [ CC'd to personal mail in case TheForge still isn't working for you. ]
>
> --
> Michael Spencer Nova Scotia, Canada .~.
> /V\
> mspencer at tallships.ca /( )\
> http://home.tallships.ca/mspencer/ ^^-^^
>
--