Here is another video of "primitive" charcoal making.  Wally does use a blue 
tarp to keep the wood pile dry until the day of the firing.  Also, all of 
the plastic buckets of water when it comes time to douse the fire.  Probably 
not the most efficient when it comes to the ratio of wood to charcoal 
realized, but think of the labor it would have taken to cover that size pile 
with mud.

Wally is a very big advocate of using charcoal to forge.

https://www.youtube.com/watch?v=I-jz0C-OgZ4


Respectfully,
Albin

--------------------------------------------------
From: "Michael via TheForge" <theforge at mailman.qth.net>
Sent: Sunday, February 21, 2016 7:04 AM
To: <theforge at mailman.qth.net>
Cc: <newenglandforge at aol.com>
Subject: Re: [TheForge] Making Charcoal

>
> Interesting.  They are currently exploring what appears to be a late 
> 15th/early 16th Century iron foundry, about 20 miles southwest of Boston. 
> The abundance of charcoal in and around the stone buildings was the first 
> tip off as to it's nature.  Apparently it was fairly common for smiths of 
> the day to "illegally" make iron for their own use, due to high taxes 
> imposed on iron being supplied by England, along with an irregular supply. 
> The site is/was well hidden a short distance from the Charles River.
> Mike
>
>
>
> -----Original Message-----
> From: Bruce . <freemab222 at gmail.com>
> To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
> Sent: Sun, Feb 21, 2016 4:35 am
> Subject: [TheForge] Making Charcoal
>
> A video on making charcoal with NO technology.  His only concessions to 
> the
> modern world are a camera and a pair of pants (for which I am
> appreciative)!  A little extreme, perhaps, but it makes it clear that it
> CAN be done by anybody with the knowledge.  A 5-minute flick, the essence
> of which you can get in about 2 min by skipping ahead.
>
> https://www.youtube.com/watch?v=GzLvqCTvOQY
>
> Bruce
> NJ
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list