[TheForge] Kaowool vs Soft Fire Brick

Saint Phlip saintphlip at gmail.com
Thu Aug 18 20:17:29 EDT 2016


Ask Oso, and maybe have him get you in contact with Atar.

On Thu, Aug 18, 2016 at 11:59 AM, Daniel Kretchmar <dan at irontreeworks.com>
wrote:

> I apologize for the misunderstanding. I was not clear about the problem.
>
>  I have built several gas forges over the years, both self aspirating and
> forced air.  The one I want to rebuild is inside a 40 lb propane tank with
> a 2 inch shell of Mizzou,  a 1 inch layer of Kaowool coated with Satanite.
> The bottom of the forge is 1 inch hardbrick.  The forge is about 18 inches
> long.  It has two burners, each with it's own squirrel cage blower, gate
> valve to control the air, and a pin valve to control the gas.  Each burner
> uses is own propane tank.
>
> The problem I am having is two fold. The hot borax has forced me to rebuild
> the Kaowool layer several times.  The borax flows down along the hardbrick
> floor and melts the kaowool along the edges.  I was wondering if Soft brick
> would prevent this. The second problem is heat. The forge ISN'T getting hot
> enough to weld larger pieces. I can weld smaller billets (12 inches long x
> 1 inch wide x 2 inches thick) but I am having trouble welding longer and
> wider pieces.  I want to make a replica of the Sutton Hoo sword, which is
> made from as many as 6 (or 12) billets, (4 billets of 7 layers each with
> twists every 4 cm and 160 layers for the outer 2 edges)  The 6 billets are
> approximately: 85 cm x 1.5 cm x 1.5 cm each.  I need to weld all six of
> them together into a single billet.  I need to weld about 6 inches at a
> time, with an overlap weld of about 2 inches each weld.  This means that I
> weld 6 inches, move down the billet 4 inches and weld the next 6 inches
> until I have welded all 85 cm.  My forge is not getting the billet hot
> enough to weld such a big billet.  I have welded it together in charcoal,
> but I want to weld it in propane
>
> Here is pic I found online:
>
> https://s-media-cache-ak0.pinimg.com/564x/f9/e2/34/
> f9e234b6f6e077265f6eee045ce55e8d.jpg
> )
>
> Suggestions are appreciated
>
> Danr
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to saintphlip at gmail.com
>



-- 
Saint Phlip

Only President Obama could double the stock market, cut the deficit by
2/3, bring
gas down under $3, get bin Laden, end 2 wars, bring unemployment down under
6%,  while fighting a government that is trying to destroy him, and still
be told he's failing as President.


Heat it up
Hit it hard
Repent as necessary.

Priorities:

It's the smith who makes the tools, not the tools which make the smith.

.I never wanted to see anybody die, but there are a few obituary notices I
have read with pleasure. -Clarence Darrow


More information about the TheForge mailing list