Here's a wild speculation. A drilled hole is different because there's
nothing in the hole to keep the surrounding metal from expanding into it.
-----Original Message-----
From: Bruce .
Sent: Wednesday, August 10, 2016 7:53 AM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] stubborn rivets
Okay, guys, it's time for one of Einstein's "thought experiments":
Take a steel plate, maybe 1/2" x 3"x3". SCRIBE a 1/2" circle in the center
of the flat so the circle will survive a little abuse. Heat the plate to
below red. Quickly measure the diameter of the circle.
Does anyone think that the circle will have got smaller? If so, please
justify your conclusion (or share whatever you've been smoking).
So, why should it be different if that scribed circle were a drilled hole?
Now, I defer to greater experience whether heating is a good means for
removing a rivet. I find that truly experienced workers usually know HOW
to do something, but often can't explain WHY it works. "How" is more
important practically.
Bruce
NJ
On Tue, Aug 9, 2016 at 9:21 PM, jerry Frost <akfrosty at mtaonline.net> wrote:
> Bingo Mike. No, heating the spring will NOT expand the hole making the
> rivet
> drop out. As Mike says the hole will shrink, this only works on rings say
> a
> nut on a bolt type situation. In the center of plate like a leaf spring
> it's
> a no go.
> removing them.
>
>
>
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
Message delivered to abrahamscloset at verizon.net
More information about the TheForge
mailing list