I'm sure this is way late in the game, but this strikes me VERY MUCH as 
a job for TIG.


On 3/10/16, 12:32 PM, Dave Mudge wrote:
> I have a client that makes large gears. He is making a brass  (or similar
> alloy ) gear that is roughly 6" wide and 36" diameter. Somehow they cut a
> gouge in the top of one tooth. Maybe 1/2" wide and 1/2" deep and a couple
> inches long. Asked me if I could silver solder the gouge. I said that one
> really can't "build up" silver solder but I happen to have a large spool of
> Silicon bronze mig wire. I am sure that I can fill the gouge with that. Any
> ideas on machine settings (Millermatic 251)
> or preheat or process? Anything will be helpful. thanks, dave
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>



More information about the TheForge mailing list