[TheForge] Arc wekding advice sought
Larry Brown
lp.brown at verizon.net
Mon Jun 1 05:00:24 EDT 2015
Maybe try pre-heating the bar to around 400 and let it cool slow. You could
also try pre and post heating with the slow cool. After that you could try a
dis-similar metals rod usually stainless with a high strength
L Brown
-----Original Message-----
From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Mike
Spencer
Sent: Sunday, May 31, 2015 7:33 PM
To: theforge at mailman.qth.net
Subject: [TheForge] Arc wekding advice sought
Trying to make something from big-truck helper spring material.
That's the more or less Z- or chicane-shaped, maybe 2"x3" in the middle,
tapering to maybe 3"x3/4" at the long end, close to 4' overall length.
I can make a very nice looking weld with 7018, DC straight polarity
(electrode negative). But the base material under the weld seems to become
exceptionally brittle, such that the whole weld bead can be easily broken
off of the base metal, leaving a fine-grained, clean gray fracture. What
appears to be a thin layer of the base metal adheres to the broken-off weld
bead.
+ Am I doing something wrong?
+ Is there a trick to welding this material?
+ Anybody know what this material is? It cuts easily on my little
bandsaw.
+ Is welding to this kind of spring alloy known to be a problem or
outright impossible without fancy industrial gear that I don't
have?
- Mike
--
Michael Spencer Nova Scotia, Canada .~.
/V\
mspencer at tallships.ca /( )\
http://home.tallships.ca/mspencer/ ^^-^^
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list