[TheForge] bolt thread repair tool
jerry Frost
akfrosty at mtaonline.net
Mon Feb 23 15:22:30 EST 2015
If you're talking about dressing an Acme thread you're talking about a different bread of cat. Square and feed screws are different for a reason, they aren't supposed to lock through stretch like nuts and bolts.
Cleaning buggered threads with a thread file literally takes a few seconds and it's right when you're finished. Trying to clean them with a triangular file is a long difficult process with questionable results.
You needed to straighten the bent screw first, then chase the threads to make the repair you mention. It'd probably be almost easier to just cut a new one. I never liked cutting threads on a lathe probably because I'm not good at it. Dad could do it in his sleep. Maybe I should've practiced more eh?
Jer
-----Original Message-----
From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Bruce .
Sent: Sunday, February 22, 2015 3:09 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] bolt thread repair tool
Well, two reasons. Because you can. And because filing threads can be a drag.
The post vise bolt I fixed with a triangular file was bent and miserable.
I tried chucking it into the lathe, but it was far too bent for that. I did spin it slowly in the lathe while using the triangular file -- that worked nicely.
Bruce
NJ
On Sun, Feb 22, 2015 at 5:45 PM, Peter Fels & Phoebe Palmer < artgawk at thegrid.net> wrote:
> I can imagine that if you have an extra tubing cutter, you could
> regrind the axle so as you rotate it it would conform to different
> thread pitches, and you could regrind the blade to the 60*(?) thread
> angle required, though it doesn’t resolve parallel tracking problems entirely.
> But why?
>
> On Feb 22, 2015, at 8:30 AM, Bruce . <freemab222 at gmail.com> wrote:
>
> I wonder whether a tubing cutter or pipe cutter would do the same.
> Might have to re-mount the cutting roller on a smaller pin so it can
> rotate slightly off-axis. I'll have to give it a try.
>
> I don't have much use for it, but I did have to clean up the pivot
> bolt on an old leg vise a few months ago and it might have come in handy for that.
> I used a triangular file, which worked.
>
> Bruce
> NJ
>
> On Sun, Feb 22, 2015 at 11:02 AM, Rob Fertner <rfertner at cox.net> wrote:
>
> >
> > I've mentioned this website before. They've recently posted about a
> > tool that may save the threads on a bolt. This may come in handy
> > with old
> stuff
> > you're repairing and you don't want modern looking bolts to spoil
> > the
> look.
> >
> > http://toolguyd.com/threadmate-tools-repair-just-about-any-threads/
> >
> > Rob
> > Wichita, KS
> >
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is http://www.shutterfly.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net Please help support this
> > email list: http://www.qsl.net/donate.html
> >
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net Please help support this email
> list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net Please help support this email
> list: http://www.qsl.net/donate.html
>
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list