OK…metal question
I have some 1”= bars of bronze that looks like Si Bronze…similar reddish color with a dull brown patina….but…
it’s really stiff when forged…about like carbon steel.
It has a really narrow forging temperature range,
from just below visible red  down to not a whole lot cooler.
It’s been frustrating to work and i’ve pretty much given up on it.
It machines OK. Polishes up nicely and brazes just fine.
I thought architectural bronze was yellower…not sure.
Any guesses?

On Nov 29, 2014, at 12:01 PM, Dave Smucker <davesmucker at hotmail.com> wrote:

Jerry,  et al,  Having lived and worked in England and Wales, do you know what it means when you ask a Lady if she has been "stuffed"?  (I know no insult was intended, just funny how English is different in the UK vs. USA.   There are many other words with different meaning dependent on if it is the USA or UK.)

No my granddaughter did NOT get stuff but she did enjoy Scrawy Boonie.  I think Scrawy Boonie is a story that will be retold many times in this family.

Dave

> From: akfrosty at mtaonline.net
> To: theforge at mailman.qth.net
> Date: Sat, 29 Nov 2014 09:05:28 -0900
> Subject: Re: [TheForge] Scrawy Boonie was in the oven
> 
> What a great bunch of typo straight lines and I missed out because I was cooking Thanksgiving dinner. Heck even Friday I was unavailable, a friend and I drove to Anchorage to do a days smithing at a friend's place. However, it's too good to let lay without getting in on so tell me Dave did your granddaughter get stuffed?
> 
> Jer
> 
> -----Original Message-----
> From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Dave Smucker
> Sent: Thursday, November 27, 2014 2:23 PM
> To: theforge at mailman.qth.net
> Subject: Re: [TheForge] Scrawy Boonie was in the oven
> 
> I am sure having a time typing today, must be the cooking wine. In the second message it should have been "didn't get cooked" 
> 
> I not the list MOM, that is a different Dave from futher south.
> 
> Dave Smucker,
> from Brasstown, NC home of John C. Campbell Folk School. (blacksmithing content)
> 
> ----------------------------------------
>> From: artgawk at thegrid.net
>> Date: Thu, 27 Nov 2014 13:00:16 -0800
>> To: theforge at mailman.qth.net
>> Subject: Re: [TheForge] Scrawy Boonie was in the oven
>> 
>> Oh my Dave!!
>> I fear you have them confused!
>> Or cooked them both!
>> Your list-mom maternal instincts seem to have failed catastrophically!
>> Frolicking in ambiguity here.
>> 
>> On Nov 27, 2014, at 12:52 PM, Dave Smucker  wrote:
>> 
>> 
>> No my grandaughter did get cooked -- but she did like Scrawy Boonie. The turkey wasn't as tough as I excepted -- but maybe the turkey was 5 years old too.
>> 
>> Dave
>> ----------------------------------------
>>> Date: Thu, 27 Nov 2014 12:13:22 -0500
>>> From: freemab222 at gmail.com
>>> To: theforge at mailman.qth.net
>>> Subject: Re: [TheForge] Scrawy Boonie the turkey
>>> 
>>> Ooh! Watch those antecedents!
>>> 
>>> I hope you didn't really mean to to say that your 5-year-old 
>>> granddaughter is in the oven!
>>> 
>>> ​Happy Turkey Day.​
>>> 
>>> Bruce
>>> NJ
>>> 
>>> On Thu, Nov 27, 2014 at 12:05 PM, Dave Smucker 
>>> 
>>> wrote:
>>> 
>>>> We are visiting our daughter and family in Madison, WI and had good 
>>>> travel getting here. I am the one fixing the turkey and my daurghter 
>>>> bought a free range turkey. Our five year old grandaughter has named 
>>>> it Scrawy Boonie. She is in the oven now and will see how she turns out.
>>>> 
>>>> Happy Thanksgiving to all on the Forge
>>>> 
>>>> Dave Smucker
>>>> Brasstown, NC
>>>> 
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>> 
>>> TheForge mail list group photo site is http://www.shutterfly.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>> 
>>> This list hosted by: http://www.qsl.net Please help support this 
>>> email list: http://www.qsl.net/donate.html
>> 
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>> 
>> TheForge mail list group photo site is http://www.shutterfly.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>> 
>> This list hosted by: http://www.qsl.net Please help support this email 
>> list: http://www.qsl.net/donate.html
>> 
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>> 
>> TheForge mail list group photo site is http://www.shutterfly.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>> 
>> This list hosted by: http://www.qsl.net Please help support this email 
>> list: http://www.qsl.net/donate.html
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
		 	   		  
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list