On our kitchen counter i used high quality , water curing urethane and it's intact after 3 years.
That's probably = to 1 month restaurant time.
On Jun 24, 2014, at 5:08 PM, crcarlo123--- via TheForge wrote:
You can have it coated with Teflon. Teflon is approved for direct food contact check with your local powder coating shop they may be able to do it
Sent from my iPhone
> On Jun 24, 2014, at 6:52 PM, "Bruce ." <freemab222 at gmail.com> wrote:
>
> Here's an MSDS for B/C PermaBlue. There might be more than one product
> under that brand name, so try to find the one you used. The supplier is
> required by law to provide it, which they usually do these days over the
> Internet, for you to print off.
> https://www.birchwoodcasey.com/getattachment/Resources/Safety-Data-Sheets/13322-13325-Perma-Blue-Paste-Gun-Blue-2012.pdf.aspx
>
> Note that that formulation contains selenium, which probably makes it a
> no-no for food use. (That's not a certainty, because it may be that the
> selenium residue on the surface would be lower than the legal threshold,
> whatever that is. Bad bet, though.)
>
> I'm not knowledgeable in the field either, but if a glossy brown or black
> finish would do, then I recommend the one finish that's generally regarded
> as safe for food: A thin coat of polyunsaturated oil, followed by heat
> (350 - 400 F for an hour works). If the metal is shiny, this will be a
> deep cocoa brown which often looks ugly. If the metal is black, it will be
> a lovely shiny black. The shine could probably be rendered to matte easily
> enough. Unfortunately, this is not a hard finish and will scratch.
>
> I note there's a discussion of this topic on Iforgeiron.com, but I didn't
> read it. There's a lot else accessible through Google. It's a real can of
> worms to be working with surfaces for restaurants. There are specific FDA
> regulations. You don't say whether these are food preparation surfaces, or
> what. I wouldn't touch something like this without a sign-off from my
> attorney and a check what my insurance will cover.
>
> Have you considered covering the surface with a transparent, food-grade
> plastic sheet, such as acrylic or polycarbonate?
> http://www.professionalplastics.com/professionalplastics/FoodProcessing-HandlingBrochure2011.pdf
>
> Bruce
> NJ
>
>
>> On Tue, Jun 24, 2014 at 5:08 PM, Wayne Ackman <stryker at vulcanpro.com> wrote:
>>
>> I've been working on a restaurant. Made them some metal countertops that
>> they wanted to have blued.
>> We used PermaBlue, which turned out decent. I then sprayed a couple coats
>> of urethane on the counters.
>> The restaurant hasn't opened yet, but someone spilled something (soda
>> supplies?) on the counter and it
>> ate right thru the finish. This has opened the concern about what kind of
>> coating we can put on the counters
>> that would furnish a food grade finish. Has anyone done this? And have
>> any suggestions?
>> Thanks for any help.
>>
>> Wayne
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.shutterfly.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list