Yeah, I did find something like that but it won't due. That stuff has to
be applied at >300 F.
I'd love to get a sample to try out but not for $100+ a pop!
I may try a wax for the purpose.
Bruce
NJ
On Wed, Dec 17, 2014 at 9:55 PM, Todd Rich <torin at panix.com> wrote:
>
>
> Plastic dip coatings:
>
> https://www.mscdirect.com/browse/tn/?searchAheadTerm=
> dip+coatings&searchAhead=true&hdrsrh=true&typahddsp=Dip+
> Coat+Coatings&navid=12104972
>
> (Shorter url for one type)
> https://www.mscdirect.com/product/details/37033263
>
> You'll also need a dip coat pot, though you might be able to cobble one
> together for cheaper:
> https://www.mscdirect.com/product/details/31734049
>
>
> On Wed, 17 Dec 2014, Bruce . wrote:
>
> Today I had a need for a product I've seen but never used myself. It
>> seems
>> to me that in years past I would get (wood) auger bits in which the
>> cutting
>> end (auger screw and cutting blades) had been dipped in some sort of
>> plastic material -- that was soft and easily removable. The idea,
>> apparently, was to minimize damage before first use.
>>
>> Does anyone know what this material was or whether it's still available?
>>
>> Bruce
>> NJ
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.shutterfly.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
>> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list