[TheForge] HF IR thermometer <$20!

Peter Fels & Phoebe Palmer artgawk at thegrid.net
Sun Dec 7 16:08:50 EST 2014


Been thinking that…at least as a way to calibrate the IR gun and my eyeball.
Since i got it, i’ve gotten better at eyeballing…sigh..


On Dec 7, 2014, at 5:29 AM, Bruce . <freemab222 at gmail.com> wrote:

Peter,
Tempil sticks might work better for you task.

Bruce
NJ

On Sun, Dec 7, 2014 at 12:56 AM, Peter Fels & Phoebe Palmer <
artgawk at thegrid.net> wrote:

> I have been forging different bronzes that of course have differing
> forging heat ranges.
> So i got one with a wider temp range, thinking it would help with that..
> But it’s sometimes slow to read, which doesn’t work with smaller pieces
> that cool quickly.
> Also, differing levels of surface oxides seem to confuse it…
> And it keeps changing it’s digital mind.
> It did better when i was keeping track of interpass temperatures and
> carbon steel tempering.
> 
> On Dec 6, 2014, at 9:33 PM, Dave Mudge <dave at magichammer.net> wrote:
> 
> Bruce, our machine shop bought one of those several years ago.
> it seems to work great. Still has the same batteries...
> dave m
> 
> On Fri, Dec 5, 2014 at 7:59 PM, Bruce . <freemab222 at gmail.com> wrote:
> 
>> Speaking of HF tools, here's one that I've found to be reliable and
>> reasonably accurate.  I've just been using mine to test pre-heat temp
>> (~400F) for welding.  I may stop by the store for a second one.
>> 
>> http://www.harborfreight.com/
>> item 69465
>> 
>> It looks like the sale is on-line only, but sometimes the stores will
> honor
>> it if you bring the ad.
>> 
>> That freebie flashlight is also a good one.  I was just using one of
> mine.
>> It has a hook on the back to hang from a nail, and switches between
>> flashlight and "lantern" modes.
>> 
>> Bruce
>> NJ
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>> 
>> TheForge mail list group photo site is
>> http://www.shutterfly.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>> 
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>> 
> 
> 
> 
> --
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> 
> NOTICE: Due to Presidential Executive Orders, the National Security Agency
> may have read this email without warning, warrant, or notice. They may do
> this without any judicial or legislative oversight. You have no recourse
> nor protection.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list