PCB transformer had a really high flash point. The old blacksmith Pete Paulson pointed that out to me long ago.
He's long since dead and i have his anvil now. The PCB oil was very effective quench oil and i used it for years
thereafter. It was thought to be pretty much inert back then.
Mmmmm...Wrong!

On Oct 25, 2013, at 7:14 PM, Rob Fertner wrote:

The museum shop had a lidded container filled with motor oil, 30W I think.
This has a lower flash point than vegetable oil.

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Peter Fels & Phoebe
Palmer
Sent: Friday, October 25, 2013 3:06 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] A different needle question

Needless to say, different oils have different flash points, but close
enough for most applications.




More information about the TheForge mailing list