[TheForge] Binders on Abrasive wheels
Charles
xlch58 at swbell.net
Sat Oct 12 13:14:51 EDT 2013
It might have been designed for a hand crank grinder where there is less speed and pressure and where its free cutting properties would be very welcome.
Charles
________________________________
From: Peter Fels & Phoebe Palmer <artgawk at thegrid.net>
To: Charles <xlch58 at swbell.net>; Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Sent: Saturday, October 12, 2013 11:41 AM
Subject: Re: [TheForge] Binders on Abrasive wheels
That's certainly what's going on here Charles.
Never saw one as soft though.
On Oct 12, 2013, at 9:20 AM, Charles wrote:
The binder varies depending on how fast of a cut the wheel is designed for. A real fast cutting wheel can have a soft binder. This means new edges are being presented constantly rather than having to wear through dull edges on the cutting particles.
Charles
________________________________
From: Peter Fels & Phoebe Palmer <artgawk at thegrid.net>
Query: I pulled an old ( don't know how old...WW2 old?) 8"X1" grinding wheel out , dug up
some centering hardware and hung it on my bench grinder.
It cuts gratifyingly quickly on hard steel!! It also wears really fast!
Looks to be around 60 grit with darkish grains in a grey matrix.
I'm wondering if the binder has gotten soft with age and it's dangerous?
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list