All aluminum used in normal production is melted in normal atmospheric
furnaces and in most cases fluxes are not used. Pouring or feeding of molten
metal is done so as to minimize the exposure to the air.  I have seen
millions of pounds cast this way.  In some of Alcoa's plants more than a 100
million pounds of finished metal is produced per month.  Alcoa used to
produce magnesium casting at their New Kensington, PA plant during WW II but
I have never seen it done.  I believe it too was melted in a normal
atmospheric furnaces but never saw it.  I do know we had a bad fire from the
burning of chips from a magnesium machining operation.  (All of this before
my time at Alcoa)  Alcoa uses a lot of magnesium today -- but as an alloying
element in a group of alloys.  The 5000 series alloys are magnesium alloys.
5182 the stuff in a beer can end is approx.. 4.5 percent magnesium.  The
body of the can is 3004.

Dave Smucker
Brasstown, NC

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Bruce .
Sent: Wednesday, October 02, 2013 5:59 AM
To: terry l. ridder; Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] a question which probably has a simple answer

I'm no expert in magnesium or its casting.  I've done a very little bit of
aluminum casting.

You are right that there's be an oxide coat on magnesium -- it's just too
reactive a metal for there NOT to be one.  Quothe Wikipedia, "It tarnishes
slightly when exposed to air, although unlike the alkali metals, an
oxygen-free environment is unnecessary for storage because magnesium is
protected by a thin layer of oxide that is fairly impermeable and difficult
to remove."

Magnesium metal conducts heat much better than does iron, and almost as well
as does aluminum.  It's ignition temperature is nearly 900 F.  Bottom line
-- it takes some doing to get a large block of aluminum up to its ignition
temperature, even if the oxide coating is penetrated.

Note that to use one of those little fire-starter magnesium blocks, you
first shave off tiny pieces with a knife.  The tiny pieces can be got to
ignition temperature moderately easily.

As to the casting question, I'd wondered the same for aluminum, which is
also quite reactive.  The answer (for aluminum) seems to be that the heat of
oxidation is dissipated through the melt so fast that it makes a negligible
contribution to the temperature of the melt, and, the oxide layer forms a
protective coat even on the melt.  I don't have numbers handy, but the
molten metal may be more thermally conductive than the solid, because the
atoms are free to move around in the melt, so, I expect, the temperature in
the crucible would tend to be fairly uniform for aluminum or magnesium.

When one casts aluminum, one should not stir the melt (much) as this exposes
the molten aluminum to air, producing slag (oxide - and maybe
nitride?)  Ideally, one would melt aluminum under an inert atmosphere (like
helium or argon, NOT under CO2 or N2, which are reactive under these
conditions).  In practice, some pretty nasty fluxes are used -- fluorides,
for example.  (In the case of aluminum and magnesium, floating ordinary
"glass" flux atop the melt may not be feasible because the glass may be
denser than the molten metal.)








On Tue, Oct 1, 2013 at 11:19 PM, terry l. ridder
<terrylr at blauedonau.com>wrote:

> hello;
>
> a 16 yrs old young man was helping with various projects to earn some 
> spending money. his parants are locked in a bitter divorce and being 
> here gives the young man time away from the combantants.
>
> we were discussing small engines and i happened to show him two 
> engines which have magnesium engine blocks. He pondered that for a 
> moment and asked the question:
>
> "What keeps the magnesium from bursting into flames like in chemisty 
> class?"
>
> his next question was:
>
> "How do they melt it to make the castings without it bursting into 
> flames?" It is melted and poured either in a vacuum or inert 
> atmosphere like argon, xenon, neon, etc.
>
> I may have known the answer at one time but have forgotten it over the 
> years. I assume that it is passivated with an oxide which has a high 
> ignition temperature.
>
> any one have a different or better answer.
>
>
> --
> terry l. ridder ><>
> ______________________________**______________________________**__
> TheForge mailing list
> Home: 
> http://mailman.qth.net/**mailman/listinfo/theforge<http://mailman.qth.
> net/mailman/listinfo/theforge>
> Help: 
> http://mailman.qth.net/mmfaq.**htm<http://mailman.qth.net/mmfaq.htm>
> Post: mailto:TheForge at mailman.qth.**net <TheForge at mailman.qth.net>
>
> TheForge mail list group photo site is http://www.shutterfly.com
> Login: 
> blacksmithblacksmith at hotmail.**com<blacksmithblacksmith at hotmail.com>
> Password: anvil
>
> This list hosted by: http://www.qsl.net Please help support this email 
> list: http://www.qsl.net/donate.html
>



--
Bruce
NJ
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list