[TheForge] lazy susan Rant
Kim George
klgeorge at kent.edu
Sat May 25 13:04:16 EDT 2013
After 40 yrs. the top pivot on the corner cabinet lazy susan wore
out. Of course you had to dismember everything to find out. Once i
had it apart i found that it was made of pot metal I went to the
hardware store only to find that you can't get parts for it.
So i had to make a patch I ship lapped a piece of steel to get the
hole in the right spot and riveted it in place and that only took 6
hrs. I hate when they discontinue parts.
--
Kim George
"Why for you try to bury me in cold,cold ground?"
Taz