[TheForge] Pendaflex file holders steel
Bruce .
freemab222 at gmail.com
Sun Jun 23 17:50:32 EDT 2013
I could test one on a grinding wheel, but they're not particularly
springy, like spring steel, so I suspect they're just A36.
On Sun, Jun 23, 2013 at 1:43 PM, Susan and Lynn Lang
<langfarm at together.net> wrote:
> Hello
> Does any one have an idea of what the Pendaflx file holder steel band is, if
> it is a higher carbon steel?
>
> lynn
>
>