Mosquito dunks? I've never heard of dunks Ron, guess I'll have to check 
Lowes after Home Depot, they're closer.

Barry: The amount of oil required to keep mosquito larve from living in 
the slack tub or any body of water is WAY too little to affect quench 
properties. All you need is a sheen, I like garlic oil, more effective 
and I LIKE garlic. A drop of Marvel Mystery Oil is good too and it 
smells like wintergreen.

I'm going to check out the dunks though, never hurts to have more than 
one trick in the bag.
Jer


On 6/5/2013 9:05 AM, Ron Childers wrote:
> Mosquito Dunks. Lowes sells them- Safe & effective per the lable...
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of barry myers
> Sent: Wednesday, June 05, 2013 12:47 PM
> To: theforge at mailman.qth.net
> Subject: [TheForge] Mosquito control in Slack Tub
>
> I think we have talked about this before, but what is the best way not
> to
> have mosquitoes in the shop?  I don't like the oil I have on the surface
> now as it on the iron and may affect my hardening.
>