There was a note on the EKmetalsmiths list about a bag of charcoal contaminated with limestone rock which exploded on the person. The suggestion was made to be wary and start checking in a bucket or sideboard any charcoal before putting it in the fire. Theirs was Cowboy Brand, but it could happen to any of them. Mike Graf