[TheForge] Sand blaster problem: hose blows off

Dan Brewer danqualman at gmail.com
Sun Jul 21 22:02:09 EDT 2013


Try cutting off 100 or so mm to get a good section of hose. The inner side of the hose should be a force fit on the barbs.  Use a screw type hose clamp and tighten until you see a slight distortion in the rubber as in it is starting to come through the slots. I have has to do this to my hf sand blaster to keep the hose on.
Dan in Auburn

Sent from my iPhone

On Jul 21, 2013, at 5:50 PM, mspencer at tallships.ca (Mike Spencer) wrote:

> 
> I have this nice little sand blaster, not what you'd want to clean up a
> ship but okay for smallish stuff -- maybe a 10 gal. pressure tank.
> Had it for a couple of years and never used it. Now I need it.
> 
> Only the hose keeps blowing off.  Very heavy hose, slides over
> ribbed nipples on hand set and feed valve, held with wire hose clamps.
> Blew off at both ends (gun and feed) at different times.
> 
> Gummed it on with silicone sealant and reset the clamps. Came off
> again. Potentially dangerous. Not good.
> 
> Is there some kind of standard hose connector for sandblasters?
> Anybody have suggestions?  Finding parts will involve a 75 mi. trip to
> the hot and sticky city.  I could use some suggestions as a starting
> point.
> 
> I could, of course, try gluing the hose on with JB Weld or Gorilla
> glue but the hose should be removable facilitate clearing any blockage
> in the valve on the bottom of the tank.  So a successful glue job
> would require excess disassembly or PITA destructive methods for
> removal when maintainance is required.
> 
> 
> - Mike
> 
> -- 
> Michael Spencer                  Nova Scotia, Canada       .~. 
>                                                           /V\ 
> mspencer at tallships.ca                                     /( )\
> http://home.tallships.ca/mspencer/                        ^^-^^
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html


More information about the TheForge mailing list