Or on the top shelf in the shop next to the HC.
Thanks James,
Dan
ferric chloride, ebay
On Feb 22, 2013, at 8:16 AM, Dan Scheid wrote:
>
> I'm stumbling though the learning process I want silver with gold
> look. But not silver and gold. So I started with nickel silver and
> brass.... big fail .. just got a small billet of nickel and silicon
> bronze fused up and patterned . the color blend and it is hard to see
> the pattern. What can be done to bring out the pattern. (patina, acid,
> whatever) and where can I get itonline?
> Thanks all Dan Scheid
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net Please help support this email
> list: http://www.qsl.net/donate.html
James Binnion
jbin at well.com
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
-----
No virus found in this message.
Checked by AVG - www.avg.com
Version: 2013.0.2899 / Virus Database: 2639/6119 - Release Date: 02/20/13
-----
No virus found in this message.
Checked by AVG - www.avg.com
Version: 2013.0.2899 / Virus Database: 2639/6119 - Release Date: 02/20/13
More information about the TheForge
mailing list