Good! Thanks Chuck
This has been a good thread, thanks all.
On Feb 17, 2013, at 9:01 AM, Chuck Robinson wrote:
For those of you interested, Evaporust is a chelating agent. Certain organic compounds are capable of forming coordinate bonds with metals through two or more atoms of the organic compound;
Cane molasses diluted in H2O is also an effective chelating agent for removing rust.
Chuck
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list