I cut a lot of circles out or 14ga and 16 ga steel. I have tin patterns (old
duct work) that I trace around with a fine marker and then cut out on a
Beverly shear. I then flatten the edge with the treadle hammer and clean up
the edges on a belt sander. Most of my cutting is done on the B3 for
something as thin as 24ga a B2 might be better, on my B3 thin material tends
to fold instead of cut. I'm sure it could be adjusted for thinner material
but then it might be too tight for the heavier stuff.
Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net
> On 9/5/2012 12:05 PM, Ron Childers wrote:
>>
>>
>> Has anyone tried a pneumatic panel cutter (like a muffler cutter) to cut
>> 5" circles in brass sheet?
>>