[TheForge] filling pipe with sand to bend
Greg Thues
thorsrevenge1 at gmail.com
Tue Nov 6 11:59:30 EST 2012
I've also done this, one of the problems I ran in to was getting the pipe to hot I melted the sand and turned it into glass which then while cooling warped the pipe
Yours sincerely
Greg Thues
On Nov 6, 2012, at 8:35 AM, Andy Gladish <anjgladish at gmail.com> wrote:
> Has anyone out there tried this?
> I've got a curved schedule 10 1 1/4" nominal railing that needs a
> transition piece between two sections- this will be a curve that changes
> direction by 15 deg. in about 11". (that's a 42" radius)
>
> I'd have to bend it around a form or make some wooden dies and use a press,
> but if it's hot it seems like it would distort unless the dies are shaped
> just right.
>
> I'm worried about distortion if I roll it cold OR hot....
>
> Then after it's done it needs to get to a brushed finish- will muriatic
> acid do that, or is it better to try to do it cold so there's less cleanup?
> Or perhaps I can just grind and sand it clean?
>
> Thanks for any ideas!
>
> --
> Andy Gladish, Element Fe Metal Studio
> Blacksmithing and Blades
> 7141 Guemes Island Road, Anacortes, WA 98221
> Phone: 360.202.1160
> Andy at ElementFe.com
>
> Visit ElementFe Metal Studio on Facebook! Just search for ElementFe and hit
> the "like" button. Lots of photos and updates weekly.
>
> Talent develops in tranquillity, character in the full current of human
> life. -Johann Wolfgang von Goethe
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge