Terry: How about just doing a specific gravity on a piece. It may not give
you a metallic analysis but it will give you a ballpark. If you actually
need a correct analysis I'm thinking you need to talk to someone with a mass
spectrometer and pay the price.
Jer
----- Original Message -----
From: "Andrew Vida" <osan at netlabs.net>
To: "terry l. ridder" <terrylr at blauedonau.com>; "Blacksmithing List
Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, January 06, 2012 1:55 PM
Subject: Re: [TheForge] a blacksmithing question and aceramic/pottery
question
>
>
> On 1/5/2012 1:49 PM, terry l. ridder wrote:
>
>> given the color of the part, we initially thought it was either copper,
>> brass or bronze alloy. the part is too light to be a copper, brass or
>> bronze alloy. using an optical microscope, an examination of the break
>> area leads me to believe that the part is a Beryllium alloy.
>>
>> why use a Beryllium alloy to make the part to being with?
>
> How about pot metal? Beryllium is very likely NOT the metal for reasons
> I will not go into here.
>
> If you can get the part into one piece, I would fill and threaded holes
> just to the limits of the threads, then make an RTV mold, shoot a wax
> and cast it in red bronze. If you think there is a critical dimension,
> spray a couple coats of well-thinned lacquer on to make up for
> shrinkage. Run a tap through the threaded areas and you are done. Fast
> and relatively painless. You can have it done in a couple of days,
> assuming you are sending the piece out to be cast.
>
> I would not over complicate the problem.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
>
> -----
> No virus found in this message.
> Checked by AVG - www.avg.com
> Version: 2012.0.1901 / Virus Database: 2109/4727 - Release Date: 01/06/12
>
More information about the TheForge
mailing list