[TheForge] a blacksmithing question and a ceramic/pottery question
terry l. ridder
terrylr at blauedonau.com
Thu Jan 5 23:04:20 EST 2012
hello;
repley intermixed below.
On Thu, 5 Jan 2012 xlch58 at swbell.net wrote:
> On 1/5/2012 12:49 PM, terry l. ridder wrote:
>> why use a Beryllium alloy to make the part to being with?
> It improves strength, but more importantly significantly enhances
> resistance to corrosion in seawater. It can be soldered, brazed and
> welded successfully, but of course is a health issue.
>
ah, yes the health issues associated with beryllium.
i have enough health issues right now and have absolutely do not want
any more health issues.
>
> Charles
>
--