Carbon steel is about 484 lb per cubic foot or 0.28 lb per cubic inch.
----- Original Message -----
From: "Dave Mudge" <dave at magichammer.net>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Monday, December 17, 2012 9:01 PM
Subject: [TheForge] How much does it weigh?
> Here is a question for anyone.
> I would like to know the combined weight of the following:
> A piece of steel plate who's dimensions are;
> 3-1/2" thick x 25" wide x 56" long
> AND
> 7 pieces of steel round stock.
> Each one is 7-1/2" diameter x 22-1/2" long
>
> Why you might ask?
> Well, some years ago I started to build a
> 300lb. +/- Kinyon style air hammer
> http://magichammer.freeservers.com/page7.html
> and
> http://davemudge.freeservers.com/Big_Hammer_Thumbs.htm
> I have all of the major components (on the pages above)
> I even have the hammer head (2 pieces of 5-1/4" sq. x 12")
> to be welded together.
> and the top and bottom flat dies 4" x 4" x 10" 4340.
> Here is how I made the flat dies for my smaller Kinyon style
> http://magichammer.freeservers.com/page51.html
> Something similar will work for the big hammer dies.
>
> Just need mounting plate for the head and guides
> and mounting plate for the cylinder and the plumbing
> and not much else.
>
> I am thinking of offering all of this for sale as a kit.
> The buyer would have to come pick it up as shipping
> charges would be outrageous
> Is anyone interested?
>
> dave m.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list