Just bought a few bags of L Brand Coke. Tried starting the same way I
normally do, rolled up newspaper in a ball, etc.
No luck, burned till the paper burned up but never got hot enough to
start the coke.
After a couple of no-go's I put some green coal on the paper as it was
burning and put the coke over that.
That worked and it burned well.
What's the trick to getting this L Brand Coke started? I'm sure a few
of you use it.
And, can you use it again after it has gone out. On my coal, I do that
after picking out the clinkers and obvious burned up stuff.
James