[TheForge] mokume- gane
Albin Drzewianowski
dski1045 at qis.net
Wed Aug 8 08:07:17 EDT 2012
There is a YouTube video sponsored by Mark Aspery that shows welding a stack
of quarters.
http://www.youtube.com/watch?v=1s71b4azPSg&feature=g-all-u
The title of the vide is part-1 but I could not find a part 2.
I believe there was an associated write up in ABANA's newsletter, "THE
HAMMER'S BLOW". possibly in the Fall 2011 issue.
D-ski
Westminster, MD
The lyf so short, the craft so long to lerne.
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net [mailto:theforge-
> bounces at mailman.qth.net] On Behalf Of Dan Scheid
> Sent: Wednesday, August 08, 2012 1:41 AM
> To: 'Blacksmithing List Sponsored by ABANA'
> Subject: [TheForge] mokume- gane
>
>
>
> I have been welding lamented steel (Damascus ) for going on over 20
years.
> And I thought of doing Mokume gane. I read that you can use US quarters as
your
> start press, heat, then weld but could not find anything about if it
needs flux.
> Anyone got a link or a book on a simple start for mokume game?
> Thanks
> Dan Scheid
>
More information about the TheForge