I wear a glove on the holding hand. Even if the piece is long and cold. Main reason is that the glove shields me from some of the piece vibration when I hit it. I don't put one on my hammer hand because I have better control.
I do use both gloves when doing twists. One hand winds up under the twist and hot scale WILL fall into the cup of the open hand below<G>.
All the best
-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Cindy and James
Sent: Thursday, March 31, 2011 12:40 PM
To: theforge at mailman.qth.net
Subject: [TheForge] gloves
On the rare occasion that I do wear gloves while forging, it is normally
on my left hand not my hammer hand. And it is normally a KEVLAR glove.
I use them when the object is too hot (and short) to hold bare handed
but long enough to be handled without tongs if the glove is used.
For those of you unfamiliar with them, it is the stuff body armor is
made from. These are knit gloves and will allow you to comfortably hold
something in the 500 degree F range. You can feel the heat immediately
thru the glove and if it is too hot, you can turn loose. The glove does
not hold heat. They are not for welding as they do not prevent sparks
at all and allow them to pass thru the glove.
I have heard these gloves are good for preventing CUTS, but I haven't
tried that.
The gloves are cheap, usually $2 to 5 per pair and last a long time,
usually 1 size fits none (they stretch). Leather gloves at the forge
are a NO- NO!
James
Paris, TX
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list