Some of the big extrusion presses use water as the working fluid. There are a bunch of problems that come from a corrosive hydraulic media but fire is not a problem :-)
The other thing that the big presses have is lots of pump capacity. The "little" press I worked with, a 750 ton had 500 HP  pump motors the big 3500 ton press had a handful of  300 or 500 hp motors. Obviously  this kind of power is only available on industrial sites. 

On Mar 19, 2011, at 1:46 PM, David E. Smucker wrote:

> The second great risk is of fire from a failure in the hydraulic hose or 
> pipe system on a press.  With HOT metal we always have present a way to 
> light off the oil mist from a leak or hose break.  