Iron bearing sand deposits around creek, stream, and river beds are easily found too.  
Sent from my BlackBerry Smartphone provided by Alltel

-----Original Message-----
From: Dan scheid <damales at pollybutte.net>
Sender: theforge-bounces at mailman.qth.net
Date: Sun, 06 Mar 2011 20:24:27 
To: Blacksmithing List Sponsored by ABANA<theforge at mailman.qth.net>
Reply-To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Subject: Re: [TheForge] Fwd: [blacksmiths] Early metal history



I think someone is blowing smoke on the start with meteors I have worked
meteors ans smelted iron I think they found some iron ore in there
copper and in the copper smelt process they found iron slag in the fire
and went from there.  I own de re metalica  and like it Dan Scheid

On Sun, 2011-03-06 at 21:34 -0600, Dave Mudge wrote:
> ----- Original Message -----
> From: Richard Ferguson
> To: blacksmiths at yahoogroups.com
> Sent: Saturday, March 05, 2011 1:20 AM
> Subject: [blacksmiths] Early metal history
> 
> 
> I have been reading a little bit on the history of metals, so I have a
> few questions.
> 
> Several sources indicated that the early iron was from meteors,
> identifiable due to the nickel content. I am having a little trouble
> imagining finding enough meteors to make things. Is this correct? What
> have they found from meteors? Where?
> 
> de re metalica was originally published in the 1556 in latin, and
> translated by Herbert Hoover (yes, the president) and his wife into
> English. Has anybody ever seen a copy of this book? Is it worth
> owning? Apparently it has many woodcut drawings of metalworking.
> 
> Any metal history books that would be worth getting? Miller publishes
> a booklet on metal history, a reprint of several articles from the
> 1960s, but it is not very detailed, and tilted towards the history of
> the Miller company.
> 
> Richard
> 
> Sculptures in copper and other metals
> www.fergusonsculpture.com
> 
> ---------------------------------------------------------------------------------------------------------------------
> 
> 
> ---------- Forwarded message ----------
> From: Iron Spirits <iron_spirits at bresnan.net>
> Date: Sat, Mar 5, 2011 at 3:14 AM
> Subject: Re: [blacksmiths] Early metal history
> To: blacksmiths at yahoogroups.com
> 
> 
> 
> 
> The book with Herbert Hoover as the translator is:
> Georgius Agricola De Re Metallica (ISBN: 1162581743 / 1-162-58174-3)
> Hoover, Herbert Clark; Hoover, Lou Henry
> 
> and is available from abebooks.com and amazon.com at a cost of $30-50.
> 
> You can read the book online with http://books.google.com/books and do
> a search for "De re metallica hoover".  Original in Latin is available
> for free in PDF format.
> 
> http://www.archive.org/details/deremetallica50agri is a link for a
> free copy of Hoover's translation in PDF, Kindle, Online and other
> formats.  I downloaded in PDF format and the PDF book looked like it
> was a exact copy, with all woodcut drawings.
> 
> Let it shine, Tom
> 
> 
> “Without continual growth and progress, such words as improvement,
> achievement, and success have no meaning.”
> 
> Benjamin Franklin
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html


______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html


More information about the TheForge mailing list