Oh I forgot silk is on that list of HCN producers too :-)
On Jun 6, 2011, at 6:22 PM, James Binnion wrote:
>
> On Jun 6, 2011, at 6:03 PM, Jerry Frost wrote:
>
>> This is the REAL downside to wearing wool as fire protection, the smoke
>> contains cyanide. This was pointed out on a smithing forum yakking about
>> this subject a few days ago. The upside is it takes a pretty serious
>> exposure to wool or hair smoke to be hazardous unless you're sensitive and
>> the smell is more than enough to clue you into taking care of the problem.
>
> Yes so does tobacco smoke, and a whole list of other organic materials will produce it when incompletely combusted. It is one of the things that kills you in fatal cases of smoke inhalation.
>
>
> James Binnion
> jbin at well.com
>
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
James Binnion
jbin at well.com
More information about the TheForge
mailing list