[TheForge] Brake Drum forge
Jay Hayes
xmas4lites at earthlink.net
Sun Jun 5 12:49:10 EDT 2011
Heat the square tube up. Forge the end round... Or, cut a piece of
plate large enough to weld over the holes in the brake drum. Cut a
square hole in the middle of the plate the size of the tube. Weld the
tube to the plate. Or cut slits down the corners if the square tube an
inch or two. Bend the sides of the tube out to make a flange. Weld or
bolt the flange to the brake drum.
On 6/5/2011 12:17 PM, Matt Gallagher wrote:
> I want to make a brake drum forge, and i have a pre made duck pot, its 2"
> square tubing, welded into a hollow tee. I want to use a brake drum as the
> firepot, but I cant think of any way to affix the tubing to the drum seeing
> as how the tubing is square and the drum has a round hole. any ideas?
>