[TheForge] black pipe
Andrew Vida
osan at netlabs.net
Sat Jul 30 13:55:13 EDT 2011
Hydrochloric acid removes it rapidly. Ferric chloride and vinegar work
more leisurely. Remove all grease and oils from surfaces prior, of course.
On 7/30/2011 12:45 PM, Mark and Sylvia Mondloch wrote:
> I have to clean the black coating off of some black pipe. I would like to
> wash it off before I sandblast and paint it. Any suggestions ? Thanks, Mark
>
> Mark and Sylvia Mondloch
> Silver Creek Pottery& Forge
> mondloch at silvercreekpottery.com
> www.silvercreekpottery.com
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list