If you leave it in the box it will collect moisture. I put it on a cookie sheet in the oven of our wood stove. After a few hours I powder it again using a bottle like a rolling pin, I then store it in an air tight container. Robert Ehrenberger Shelbyville, Mo. eforge at centurytel.net