[TheForge] Forge welding
James Binnion
jbin at well.com
Tue Jul 26 15:35:44 EDT 2011
On Jul 26, 2011, at 12:19 PM, Mike Spencer wrote:
> That powder sticks to hot iron real good, melts quickly at orange heat
> and wicks into joints pretty well. Doesn't foam and froth. And
> it doesn't seem to pick up water from the air, either, so it keeps
> indefinitely.
Michael,
I agree with the first part but in my experience it will definitely suck moisture out of the air over time. How fast I guess will depend on your local humidity.
James Binnion
jbin at well.com