Sounds interesting Paul, certainly worth a try. Pam puts out a garlic, olive
oil spray or used to anyway.
As far as violent outgassing if too tightly capped, no worry here, none of
us are too tightly capped on a good day and we tend to outgas a little at a
time nearly continusously. <grin>
Jer
----- Original Message -----
From: "Paul Tomlinson" <paul at fongkong.net>
To: <TheForge at mailman.qth.net>
Sent: Friday, July 06, 2012 2:48 AM
Subject: [TheForge] Rust-proofing mild steel - accidental discovery
>
> Hi Guys/Gals,
>
> Greetings from sunny^b^b^b^b^brainy Jamaica! I have been lurking on
> and learning from this list for a long time, from even before I went
> to Campbell in 2001 to do a week long introductory BS course with Dan
> Tull.
>
> I really wonder if this will work for anybody else, but it is working
> on everything I have used it on, and in the rainy season it is so
> humid that everything gets mouldy or rusts like blazes!
>
> Anyway after our last big hurricane my favourite forged sculpture was
> really rusty and I had an olive oil and garlic salad-spray close at
> hand ...! It has not rusted since, its been years, and I handle it
> regularly to check if its started to rust yet!
>
> I now use garlic laced olive oil for anything I don't want to rust -
> and none of them do.
>
> Having never tried this on clean metal I do not know if it will keep
> all rust off, but, a surface with a fine coating of rust ends up with
> a slightly brown patina which I rather like.
>
> I hope somebody finds this useful,
>
> Paul
>
> PS - I make garlic olive oil by slicing garlic into a bottle of oil.
> By the way DO NOT CAP THE BOTTLE TIGHTLY AS THERE IS A REACTION THAT
> RELEASES LOTS OF GAS OVER A WEEK OR TWO!
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
>
> -----
> No virus found in this message.
> Checked by AVG - www.avg.com
> Version: 10.0.1388 / Virus Database: 1516/3751 - Release Date: 07/08/11
>
More information about the TheForge
mailing list