[TheForge] Gun bluing & browning (book)

Robert J Hill wskewinu at mac.com
Thu Jan 13 23:46:30 EST 2011


I bought this book from Brownell's, in stock, no backorder.  It is  
pretty old and full of various recipes.  I prefer the pre made  
solutions to making my own.  Just seems easier.  They also have a ton  
of metal finishing products.  Be sure to get their big catalog.   
There's a lot of cool stuff in it.
Rob

Other chemicals to look into;

http://www.epi.com/pages/metal-antiquing-oxidizers

http://www.birchwoodcasey.com/antiquing/options.html


On Jan 13, 2011, at 04:32, Bruce Freeman wrote:

Mark,

The book is "Firearm Blueing and Browning"
by R.H. Angier
The Stackpole Co., Harrisburg, PA, c. 1936

Try bookfinder.com

While looking through the TOC, I noticed something interesting:  The
author doesn't seem to distinguish bluing from browning!  Section III
is "Prep. of Blueing and Browning Solutions", with no distinction
between them, and Section IV is >>Brownes ("Blues") and working
instructions<<<

Now, I'm no firearms expert, but I was always of the understanding
that the color brown was somewhat different from the color blue!

On Wed, Jan 12, 2011 at 11:40 PM,  <williamsiron at comcast.net> wrote:
>
>
> Bruce,
>
>
>
> Can you tell me who is the author or who the publisher was? I can  
> look it up at a technical bookstore and, maybe, find a copy.
>
>
>
> BTW I missed seeing you at Gichner's.
>
>
>
> Mark Williams
>
> Snow Hill, Maryland
> ----- Original Message -----
> From: "Bruce Freeman" <freemab222 at gmail.com>
> To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Tuesday, January 11, 2011 3:03:54 PM
> Subject: [TheForge] Gun bluing & browning (book)
>
> I have a book by the title above.  I've glanced through it but never
> had occasion to really delve into it.
>
> I'm retired now, and if someone is interested in going to the trouble
> to try some of what it recommends, I'd happily assist as an "advisor"
> -- namely, owner of the book, owner of a scanner, and a chemist by
> profession.  (I'm not a toxicologist, but can probably give you
> adequate warning if you're likely to be poisoning yourself -- and how
> to avoid doing so.)
>
> I suspect that do-it-yourself gun bluing or browning could be much
> cheaper than buying commercial products.  The catch is time and
> energy.  Accordingly, this approach is not for everybody.
>
> I'd be interested in the outcome -- maybe you could post before and
> after photos of your experiments.  (I would not suggest trying
> formulations on expensive objects until you are quite confident of
> them.)
>
> Anyone interested?
>
> --
> Bruce
> NJ
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html



-- 
Bruce
NJ
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list