I took my sword to my local gun smith. he has a salt bluing tank/system. 
cost me 3 bucks to have it blued. I did all the prep work and took the 
blame if it came out like crap. It came out fantastic.  for things like 
this having the right equipment really makes a difference
Dan Scheid

On 1/11/2011 9:23 AM, FireWorks PDX wrote:
>   I've seen  some great examples of iron finished with gun bluing and some descriptions of sealing it in linseed oil or lacquer, but, after going to buy some gun blue, I've come to discover that applying gun blue in an even coat without bathing the iron in a tank of it (as gunsmiths apparently do), not to mention that it's challenging to find a place that sells the amount necessary to seal a larger project (in this case a welded table frame). Thoughts?
>
> Thanks,
>
> Mark Novak
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list