SOFA did one a couple years ago at the start of their conference.
It took a couple or more tries to get the top to weld and then maybe it was
not the best
They built tongs to roll it in the fire and to bring it out.
I believe they had 4 strikers pounding on it
I think that Tom's problem was that he tried to use an improvised forge. If
you have a real forge big enough to bring an anvil up to welding heat it
would be a good start. You also need some sort of crane to move the hot
anvil into position. It would be exciting, be sure to make a video.