Hey Ron,
Haven't had this experience but have read that it is a danger and have annealed the few I've welded onl.
Jeff
Sent from my iPad
On Aug 19, 2011, at 8:34 AM, "Ron Childers" <ron at munlaw.net> wrote:
> A friend said he was trying to weld on a ball bearing and it exploded.
> Has anyone else had this experience? I anneal the bearing first and
> since I'm welding it to mild steel I think it should be preheated.
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list