[TheForge] to heat treat or not to heat treat... that is my question.

peter fels & phoebe palmer artgawk at thegrid.net
Thu Oct 28 23:37:03 EDT 2010


Excellent Jason..Keep a lid handy anyway.
I learned that the hard way.
I kinda owe you an apology for assuming
you knew less than you obviously do.

Them roofing tar buckets are a mainstay around here.

On 10/28/2010 7:54 PM, Jason Nass wrote:
> I know better than that Peter. I rounded up about 4.5 gallons of used motor
> oil from the maintainance garage up the street and stuck it into a metal
> roofing tar bucket I had laying around.
>
> Jason Nass - MacTalis Ironworks
> me at wargoth.com
>
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of peter fels&  phoebe
> palmer
> Sent: Thursday, October 28, 2010 10:19 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] to heat treat or not to heat treat... that is my
> question.
>
> Not enough volume to avoid a flash fire and the smoke from drain oil is hard
> on your lungs, respectfully.
>
> On 10/28/2010 1:20 PM, Mark A. Pesetsky wrote:
>> Do an oil change on your car and save the oil for the job.
>>
>> -----Original Message-----
>> From: theforge-bounces at mailman.qth.net
>> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jason Nass
>> Sent: Thursday, October 28, 2010 3:44 PM
>> To: 'Blacksmithing List Sponsored by ABANA'
>> Subject: Re: [TheForge] to heat treat or not to heat treat... that is my
> question.
>> Good point... guess I'm on the search for random oil... LOL
>>
>> Jason Nass - MacTalis Ironworks
>> me at wargoth.com
>>
>>
>> -----Original Message-----
>> From: theforge-bounces at mailman.qth.net
>> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of peter fels&
>> phoebe palmer
>> Sent: Thursday, October 28, 2010 3:18 PM
>> To: Blacksmithing List Sponsored by ABANA
>> Subject: Re: [TheForge] to heat treat or not to heat treat... that is my
> question.
>> Normalize at least...
>> Tho i'm no metallurgist,
>>     It'd be nice to harden and temper it as not all metal work
>> operations are hot.
>>
>> On 10/28/2010 11:49 AM, Jason Nass wrote:
>>> Just finished up an anvil bick of 4140. I'm not overly familiar with
>>> using it for tools, so I am undecided whether to heat treat it and
>>> risk it being to brittle to deal with impact, or just leave it
>>> normalized. I'd imagine that being it is a high strength alloy, it
>>> should hold up to having hot steel hammered around it, especially
>>> being as I ain't gonna be using no 12# sledges on it. What thoughts
>>> might you metallurgist types have on the matter?
>>>
>>> Jason Nass - MacTalis Ironworks
>>> me at wargoth.com
>>>
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is http://www.photoworks.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net Please help support this
>>> email
>>> list: http://www.qsl.net/donate.html
>>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net Please help support this email
>> list: http://www.qsl.net/donate.html
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net Please help support this email
>> list: http://www.qsl.net/donate.html
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net Please help support this email
>> list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list