[TheForge] cortisone and rust

peter fels & phoebe palmer artgawk at thegrid.net
Thu Oct 28 15:06:12 EDT 2010


Ah...thanks again Clyde!

On 10/28/2010 7:21 AM, Clyde Wynia wrote:
> I sometimes get some rust washing off to bare metal if I forget to wash the
> piece over night. I usually rinse off after an hour. At that time I have a
> pretty good rust started and rinsing doesn't was it off.
>
>
> Peter wrote:
>
> Clyde, any idea of what would cause your excellent rust formula to
> seemingly work well, but then areas of the patina float off when sprayed
> down with a hose the next day?
> It's possible that my preparatory alcohol flush  caused some oils to
> rise up out of the clean plywood the piece was set on for the alc scrub
> down...(that's the bottom surface that has the problem) . But that's all
> i can think of. It was thoroughly wire brushed.
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list