[TheForge] Pipe bending

Bob Willman blcksmth at wcnet.org
Wed Oct 20 12:22:02 EDT 2010


	Pack it with DRY sand and bend hot - romove sand when cold.


Bob Willman
The Eagle's Anvil
WB8NQW
Bowling Green, Ohio

The democracy will cease to exist when you take away from those who are
willing to work and give to those who would not.

Thomas Jefferson
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Dan Armstrong
Sent: Wednesday, October 20, 2010 11:36 AM
To: theforge at mailman.qth.net
Subject: [TheForge] Pipe bending

I need to bend a length of 1 1/4" pipe about 45 degrees as part of a
handrailing. Any ideas on how to best do that without access to a Hossfeld
or other non-crimping process ?

In the past I necked down and then upset (to create a kind of bubbley
effect) and then bent there. It worked and looked interesting. This time
when I tried it, and after doing a bunch of other work to the pipe, the
necked down part was too tired and a tear started which couldn't be salvaged
(I tried).

Thanks for any appropriate info.

Dan A.
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html




More information about the TheForge mailing list