Lead's probably cheaper when you compare fuel costs for melting the iron.
Jer
----- Original Message -----
From: "peter fels & phoebe palmer" <artgawk at thegrid.net>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, October 14, 2010 5:52 AM
Subject: Re: [TheForge] Anvil repair workshop in NJ
> Gee Jason;
> Never saw one like that..only solid cast iron.
> Without a tool steel face they are fine door stops.
> Seems odd..isn't lead shot more expensive than cast iron?
>
> On 10/13/2010 1:43 PM, Jason Nass wrote:
>> My experience with chinese made anvils is that they tend to be cast
>> hollow and use lead shot to get the weight... I stay as far away from
>> them as possible.
>>
>> Jason Nass – MacTalis Ironworks
>> me at wargoth.com
>>