[TheForge] why doesn't cast iron oxidize and burn in the same way?(was: oil/wax finish, blackened steel)
Bruce Freeman
freemab222 at gmail.com
Mon Nov 1 23:10:47 EDT 2010
Andy,
Yes, when you "burn" steel, the iron is oxidizing.
I'm not sure I follow the question about cast iron. It certainly will
oxidize (rust). Does this question refer to cutting with an oxygen
stream?
On Mon, Nov 1, 2010 at 2:29 PM, Andy Gladish <gladish at cablerocket.com> wrote:
> I was teaching metal fab for a wind turbine building class this past week
> (see www.scoraigwind.com ) this past week, and in the middle of a run of
> torch work got asked a number of times, what is actually going on when you
> burn steel...is the iron oxidizing? If so, why doesn't cast iron oxidize and
> burn in the same way?
> Anyone want to field that one?
> Andy G.
--
Bruce
NJ
More information about the TheForge
mailing list