An old lug wrench makes a good one if the pritchel is big enough
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of William Bohl
Sent: Tuesday, March 16, 2010 10:43 PM
To: 'Blacksmithing List Sponsored by ABANA'
Subject: Re: [TheForge] Holdfast Thanks
I too use holdfasts for woodworking and believe that the fit is pretty key.
The woodworking ones I use are made from 3/4 inch mild steel round bar but I
was limited to the size of the pritchel hole for the one for my anvil. My
website has some photos of some woodworking holdfasts which I use a lot.
Although the anvil holdfast clamps well I don't find myself using it much.
I like the idea of using a chain across the anvil with a weight.
Bill
Denver
http://www.bohlfamily.com/billmain.html
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Bob Smolen
Sent: Monday, March 15, 2010 11:06 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Holdfast Thanks
I use a similar holdfast for woodworking. When I take the board out from
under the holdfast and forget to gently lower the holdfast to the bench,
just the weight of it causes it to jam to the bench top. I cant pull the
holdfast out without first hitting the back of it. I think the hole needs to
be close to the diameter of the holdfast. If there is a lot of slop, more
difficult to get a good hold.
Bob
----- Original Message -----
From: "William Bohl" <bohlb at comcast.net>
To: "'Blacksmithing List Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Monday, March 15, 2010 9:52 PM
Subject: Re: [TheForge] Holdfast Thanks
> This link will take you to an example of an anvil holdfast
> http://www.bohlfamily.com/images/hf4.JPG
>
> Bill
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Mark A. Pesetsky
> Sent: Monday, March 15, 2010 5:36 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] Holdfast Thanks
>
> Any of you want to share pics of the different designs among the group?
>
> Thanks
> Mark
>
> ________________________________
>
> From: theforge-bounces at mailman.qth.net on behalf of Noah Morris
> Sent: Mon 3/15/2010 4:57 PM
> To: The Forge
> Subject: [TheForge] Holdfast Thanks
>
>
>
>
> Thank you all for you advice. I really like the chain holdfast with the
> treadle board at the end I think I am going to go for that one. And I will
> keep y'all posted as to the results.
>
> Thanks again, guys.
>
> _________________________________________________________________
> The New Busy is not the old busy. Search, chat and e-mail from your inbox.
>
http://www.windowslive.com/campaign/thenewbusy?ocid=PID27925::T:WLMTAGL:ON:W
> L:en-US:WM_HMP:032010_3
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com <http://www.photoaccess.com/>
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net <http://www.qsl.net/> Please help
> support this email list: http://www.qsl.net/donate.html
>
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
----------------------------------------------------------------------------
----
No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.436 / Virus Database: 271.1.1/2748 - Release Date: 03/15/10
07:33:00
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
****************************************************************************
********
This footnote confirms that this email message has been scanned by
PineApp Mail-SeCure for the presence of malicious code, vandals & computer
viruses.
****************************************************************************
********
************************************************************************************
This footnote confirms that this email message has been scanned by
PineApp Mail-SeCure for the presence of malicious code, vandals & computer viruses.
************************************************************************************
More information about the TheForge
mailing list