Don:
2 things have been firmly established.
1. There is only one, truly right way to do this.\
2. We aren't going to do it that way.

PlumDon at aol.com wrote:
> The Israeli guys at the ABANA conference harden their air hardening steels  
> by taking them to critical temp and burying them top down in vermiculite 
> leaving  about an inch of the working end exposed to harden. 
> 
> In a message dated  6/21/2010 7:59:11 P.M. Eastern Daylight Time, 
> artgawk at thegrid.net  writes:
> 
> I think EA Chase effected the tempering step by burying 
> the cutting  edge in a fat piece of hot steel.
>  
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list