[TheForge] Metal Prices!

ries ries at riesniemi.com
Sun Jun 20 17:02:58 EDT 2010


You guys are a bit confused about this-
First- there are two basic processes used in the USA to make steel-
one is to take iron ore, or taconite, and, using the BOF, create steel  
from it.
In this process, for the last 80 years or so, a small percentage of  
scrap steel has been mixed in, but the majority of the melt is virgin  
ore.
Second- EAF, or Electric Arc Furnaces, are used to melt scrap steel,  
which is then tweaked by adding various other metals and chemicals,  
and, usually, made into steel using the continuous casting technique.
Nucor, an entirely US owned company, built its first EAF to make steel  
from scrap, in Darlington South Carolina, in 1968.
So, for the last 42 years, steel has been made IN THE USA, using 100%  
scrap.

The reason chinese steel is bad is not whether or not its made from  
scrap- its all in the quality control.

Nucor is now the second largest steel company in the USA, and all  
their mills use EAF to make steel from scrap. I would be amazed if any  
blacksmith has not ended up with a fair amount of Nucor steel at  
various times- it is sold all over the USA.
Its perfectly good stuff.
So making it from scrap has nothing to do with quality.

Nucor will probably make between 20 and 25 million tons of steel this  
year, in the USA. They have over 200 facilities, of which something  
like 20 are mills, and total employees, for the whole country, are  
about 11,000.
In the old days, ONE mill in PA or Ohio would have that many  
employees- many would have more.
US Steel, the big, famous company, peaked in its US production at 35  
million tons, in 1953, and it took them something like 200,000 workers  
to do that.
Nucor is currently running their mills at about 75% capacity.
Its quite possible that Nucor, with its 11,000 employees, could crank  
out as much steel today as US Steel did in 53 with 200,000 plus workers.

That has nothing to do with the chinese, or our lack of an industrial  
policy, or offshoring manufacturing- its all about automation and  
efficiency.

Its a FACT that we are only selling six million tons a year of scrap  
to the Chinese.
The chinese make most of their steel from ore, they imported 380  
Million tons of ore last year. Much of it from Australia.
They make plenty of their own scrap, believe me- they made 470 million  
tons of steel in china in 2007, well over 4 times our production, and  
the vast majority of it is used in china- they are building enormous  
new dams, bridges, railroads, skyscrapers, stadiums, and more.

We dont make anywhere enough scrap, as a country, to supply China-  
there are only 300 million of us, after all.

I still maintain MOST US scrap steel is used in US steel plants to  
make steel here.
And we make 80% of our own steel needs here at home.
We dont import that much. 20% or so, and a good piece of that is high  
quality stuff from Japan, Germany, and Brazil.
It is absolutely true that the Russians, the Indians, The Germans, and  
the Chinese all have been buying steel companies in the USA- but far  
from sourcing the steel from outside countries, all of them have been  
spending BIllions of dollars to rebuild older US mills, and to build  
brand new steel mills in america.
Currently under construction or recently finished in the USA are over  
20 billion dollars worth of new steel mills.
Thyssen Krupp, the german company, is right in the middle of a new $5  
Billion mill in Alabama.
The Indians are building a couple of new mills in the USA, including a  
state of the art Direct Reduction mill in northern Minnesota.

Its a bad thing that our mills are owned by foreigners, but, unlike  
american financiers, they are putting their money where their mouth  
is, and investing in America. Now, if only we could do that too..

ries





On Jun 20, 2010, at 9:33 AM, Jerry Smith wrote:

John,

I live in steel valley and almost no steel is produced here any more.  
Many of the companies in the states are owned by foreign companies and  
those companies are building new mill in Mexico to produce steel for  
the Mexican auto manufacturing market. Watch the NHK news on PBS you  
may find out some interesting things, such as Nippon steel is building  
a new mill in Mexico.

China is now producing a record number of I beams and rail road rails  
at the moment, as well as building new coal fired electrical plants  
something like 1 or 2 going online every month, all for domestic use.  
All of these industries take steel and a lot of it.

If China, or Arcelor Mettal or the Russians or many other companies on  
the planet are producing lots of steel, where are they getting steel  
to recycle from? I already know the answer.

We hear a lot about the industry in the states and the over all  
quality of the product, but this is a very large planet in which China  
and India are growing incredibily fast and those markets need lots of  
product.

I could go on and on, but in the states we are own worst enemies and  
steel production in my area has been rock bottom since the late 60s  
and early 70s, so people need to look back 40 plus years, not 20 as  
some data suggests.

Jerry






________________________________
From: John Allen <countrymetals at gmail.com>
To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Sent: Sun, June 20, 2010 7:51:17 AM
Subject: Re: [TheForge] Metal Prices!

US steel is supposedly only to contain a maximum of 25% wrap. China is  
more
like 80%. I know when I worked in a large steel supply house, the made  
in
China steel ALWAYS cracked or even broke when we bent it. The made in
America stuff was always nice stuff to work with.

The steel yard sent all of their scrap to a large scrap yard, the  
biggest
one in NJ and then it got loaded on ship bound for china.

On Jun 18, 2010 11:02 PM, "ries" <ries at riesniemi.com> wrote:

On Jun 18, 2010, at 5:16 PM, Jerry Smith wrote:


Yes I have, but the local scrap yard guys are sell...
Jerry- you sure about that?
The USA, as a whole, makes about half the steel we make from scrap.
Depends on the economy, of course, how much steel we make here in the
USA- before a couple of years ago, when things were booming, we were
making a bit over 100 million tons a year of steel domestically.
Last I heard, these days its more like 80 million tons.
Of those 80 million tons, about half, thats FORTY MILLION TONS of
steel is made right here in the USA from scrap steel.

Nucor likes to keep on hand, at each of its 20 or so mini-mills, about
a million tons of scrap at any given time.

What this means is that our export of scrap to China is a lot less
than the "common wisdom" thinks it is.
In 2009, the best figures I can find indicate we sold about 6 million
tons of scrap to China, the most ever.

So- domestic use of scrap to make new steel-
40 million tons.
export of scrap to China-
6 million tons.

4 times out of 5, your scrap is going to US mills instead of China...

ries






You guys seeing that sort of [extreme] price increases?



Wes (aka William the Tinker)




---...

Ries Niemi
Industrial Artist
http://www.riesniemi.com/




_________________________________________...

TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qt...
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html

Ries Niemi
Industrial Artist
http://www.riesniemi.com/







More information about the TheForge mailing list